Thermal Annealing Impact on Optical Properties of Spin-coated P3HT: CdS Thin Film
| dc.contributor.author | Zakaria, Nabila Anis | |
| dc.contributor.author | Azmi, Mohd Syahriman Mohd | |
| dc.contributor.author | Naning, Fatin Hana | |
| dc.contributor.author | Capan, Rifat | |
| dc.contributor.author | Mohamad, Syed Abdul Malik Syed | |
| dc.date.accessioned | 2025-07-03T21:17:51Z | |
| dc.date.issued | 2023 | |
| dc.department | Balıkesir Üniversitesi | |
| dc.description.abstract | Polymers are flexible materials that can be easily processed and are formed into a thin film by several methods such as spin-coating, dip-coating, film-casting, and printing. The spin coating method has been extensively utilized in fabricating solution-prepared organic/inorganic electronic devices, this technique is positively efficient in generating thin film apart from being a flexible method to execute. In this study, poly(3-hexylthiophene) (P3HT) material is selected as polymer and cadmium sulphide (CdS) as nanoparticles to produce a hybrid nanocomposite thin film through the process spin-coating method. The P3HT and cadmium ion solution were used to fabricate a thin film onto a quartz glass substrate at a spin speed of 500 rpm for 10 seconds. This spin-coated thin film was heated at different temperatures such as 40°C, 80°C, 120°C, and 160°C for optical properties using a UV-Vis spectrophotometer. The UV-Vis absorption spectra of P3HT: CdS indicated absorption peaks in the UV region, which were ascribed to the band gap of the P3HT: CdS thin film. Our results showed that the optical properties of the P3HT: CdS be contingent on the annealing temperature. The film at room temperature yielded a band gap value of 1.98 eV, at 40°C it resulted in 1.99 eV. The band gap value was increased when annealed at 80°C with 2.02 eV. Annealing temperatures were then raised to 120°C and 160°C, leading to band gap values of 3.11 eV and 2.80 eV respectively. © 2023, Universiti Pendidikan Sultan Idris. All rights reserved. | |
| dc.description.sponsorship | Ministry of Higher Education, Malaysia, MOHE, (2020-0257-104-02) | |
| dc.description.sponsorship | Ministry of Higher Education, Malaysia, MOHE | |
| dc.identifier.doi | 10.37134/jsml.vol11.sp.9.2023 | |
| dc.identifier.endpage | 97 | |
| dc.identifier.issn | 2462-2052 | |
| dc.identifier.issue | Special Issue | |
| dc.identifier.scopus | 2-s2.0-105001563037 | |
| dc.identifier.scopusquality | N/A | |
| dc.identifier.startpage | 81 | |
| dc.identifier.uri | https://doi.org/10.37134/jsml.vol11.sp.9.2023 | |
| dc.identifier.uri | https://hdl.handle.net/20.500.12462/21067 | |
| dc.identifier.volume | 11 | |
| dc.indekslendigikaynak | Scopus | |
| dc.language.iso | en | |
| dc.publisher | Universiti Pendidikan Sultan Idris | |
| dc.relation.ispartof | Journal of Science and Mathematics Letters | |
| dc.relation.publicationcategory | Makale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı | |
| dc.rights | info:eu-repo/semantics/openAccess | |
| dc.snmz | KA_Scopus_20250703 | |
| dc.subject | CdS nanoparticles | |
| dc.subject | optical properties | |
| dc.subject | P3HT | |
| dc.subject | spin coating | |
| dc.subject | Thermal annealing | |
| dc.title | Thermal Annealing Impact on Optical Properties of Spin-coated P3HT: CdS Thin Film | |
| dc.type | Article |